铜箔中间层对铝/钢异种金属激光对接焊接头质量的影响

杨旭东;石岩;刘佳   

  1. 长春理工大学机电工程学院
  • 发布日期:2014-07-20

Effect of Cu Foil on Laser Butt Welding Quality of Aluminum/Steel Dissimilar Metals Joint

YANG Xudong;SHI Yan;LIU Jia   

  1. School of Electromechanical Engineering, Changchun University of Science and Technology
  • Published:2014-07-20

摘要: 采用添加铜箔中间层方式对08Al钢与5083铝合金进行激光对接焊试验,试验过程中将光斑偏向钢一侧。以焊缝成形质量为标准,获得了最优的焊接工艺参数组合。采用金相显微镜和扫描电镜分析铜箔中间层对界面处熔合情况、元素分布及焊缝各区域微观组织结构的影响。研究结果表明,当光束偏移距离为0.4 mm,离焦量为0 mm,激光功率为2 kW,焊接速度为10 mm/s,保护气He流量为15 L/min时焊缝表面连续、平整,无飞溅、夹杂和咬边等缺陷,背部熔透均匀,焊缝成形质量最佳。添加的铜箔中间层形成铝和钢之间的过渡桥梁,使对接面处铝/钢物理性质过渡平缓,有效降低了界面处液态金属的温度梯度和热传递速度,液态熔池的高温停留时间延长使得下部金属获得更多的有效热量,熔化量显著增加。焊缝截面形状从T形转变为两头宽中间窄的近似X形,界面处熔合线呈现不规则的弯曲状,铝/钢相互咬合,连接紧密。铜箔中间层抑制了Al元素向钢侧焊缝的扩散,铁素体晶粒内第二相粒子明显减少。铝/铜/钢接头断裂形式为解理断裂和准解理断裂相混合,界面处生成了(Fe, Cu)4Al13、(Fe, Cu)2Al5和CuAl2脆性相,是限制接头强度提升的主要原因。

关键词: 激光焊;铝/钢;铜箔;脆性相, 车辆稳定性, 等效锥度, 轮轨接触关系, 踏面设计

Abstract: Laser butt welding is held on 08Al steel to 5083 aluminum alloy with Cu foil interlayer. Laser spot is shifted to the side of steel during the test. Optimal process parameters are determined by analysis and contrast of the welding formation. The influence of Cu elements on interface fusion, elements distribution and microstructure of weld zone are analysised by using optical microscope and scanning electron microscope. The results show that welding quality is best while the beam offset distance is 0.4 mm, defocusing amount is 0 mm, laser power is 2 kW, welding speed is 10 mm/s, flow of He gas is 15 L/min. The copper foil interlayer forms a bridge between aluminum and steel, which makes the transition of the physical properties of aluminum/steel more smooth and effectively reduced the temperature gradient and heat transfer rate at the interface of the liquid metal, while the residence time of high temperature of the molten pool is extended, so that the lower metal obtains more effective heat and the melting increased significantly. The section shape of weld changes from “T” to approximate “X”. The interface fusion line is irregularly curved, aluminum and steel meshed and connect closely. The cu foil inhibits the diffusion of al to the side of steel, and the second phase particles within ferrite grains significantly reduced. Aluminum/copper/steel joint combines cleavage fracture and quasi cleavage fracture. The brittle phrase of (Fe, Cu)4Al13、(Fe, Cu)2Al5 and CuAl2 are formed at the interface which is the main reason for the low improvement of joint strength.

Key words: laser welding;aluminum/steel;copper foil;brittle phase, Equivalent conicity, Tread design, Vehicle stability, Wheel-rail contact relationship

中图分类号: