Cr-Mo-V钢焊缝金属韧脆转变行为与晶粒协调变形的关联机制

窦贵山1, 曹睿1, 乔小丽2, 蒋勇3, 李义民2, 陶彦文2, 张克静3, 李金梅4, 王岑2, 林巧力1   

  1. 1. 兰州理工大学材料科学与工程学院 兰州 730050;
    2. 兰州兰石重型装备股份有限公司 兰州 730050;
    3. 四川大西洋焊接材料股份有限公司 自贡 643000;
    4. 兰州兰石检测有限公司 兰州 730050
  • 收稿日期:2025-12-03 修回日期:2026-05-15 发布日期:2026-11-20
  • 作者简介:窦贵山,男,1995年出生,博士研究生。主要研究方向为焊缝金属的断裂韧性。E-mail:dougs0615@163.com;曹睿(通信作者),女,1977年出生,博士,教授,博士研究生导师。主要研究方向为新材料、异种材料的焊接性、强韧性、腐蚀、变形、损伤及断裂行为等。E-mail:caorui@lut.edu.cn
  • 基金资助:
    甘肃省重点研发计划(23YFGA0057)、甘肃省拔尖领军人才、中央引导地方科技发展专项(24ZYQA054)、国家自然科学基金(52175325)和甘肃省科技重大专项(24ZD13GA018,23ZDGA010,22ZD6GA008)资助项目。

Correlation between the Ductile Brittle Transition Behavior and the Coordinated Deformation of Adjacent Grains of Cr-Mo-V Steel Weld Metal

DOU Guishan1, CAO Rui1, QIAO Xiaoli2, JIANG Yong3, LI Yimin2, TAO Yanwen2, ZHANG Kejing3, LI Jinmei4, WANG Cen2, LIN Qiaoli1   

  1. 1. Department of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050;
    2. Lanzhou Ls Heavy Equipment Co., Ltd., Lanzhou 730050;
    3. Sichuan Atlantic Welding Materials Co., Ltd., Zigong 643000;
    4. Lanzhou Ls Testing Technology Co., Ltd., Lanzhou 730050
  • Received:2025-12-03 Revised:2026-05-15 Published:2026-11-20

摘要: 2.25Cr1Mo0.25V钢因其优异的高温性能、抗回火性能以及持久性能,被广泛应用于临氢设备和高温高压管道,其焊缝金属在焊接过程中易出现微观组织不均匀以及韧脆转变温度较高等问题,这些问题直接影响焊接结构件在低温或变载条件下的安全性与可靠性。因此深入研究其焊缝金属的组织调控与韧性改善机制,对该材料在大型设备中长期稳定运行具有重要意义。利用扫描电子显微镜(Scanning electron microscope, SEM)和电子背散射衍射(Electron back scatter diffraction, EBSD)表征焊态(As-welded, AW)与两种焊后热处理(Post weld heat treatment, PWHT)态(705 ℃×8 h (PWHT.MIN)和705 ℃×32 h (PWHT.MAX))下焊缝金属的微观结构;并通过高低温环境下的夏比冲击试验检测了焊缝金属的冲击韧性。结果表明:焊态试样的显微组织主要由块状铁素体和粒状贝氏体组成,表现出微观结构不均匀性和晶粒间变形不协调性,常温下冲击功低于10 J;焊态试样200 ℃下保温20 min后,显微组织中出现铁素体,冲击功随之提高到90 J。但经过焊后热处理之后,试样的显微组织以铁素体组织为主,室温下冲击功提高到200 J。AW、PWHT.MIN和PWHT.MAX试样的韧脆转变温度分别为158 ℃、-30 ℃和-40 ℃。随着回火时间的延长,晶粒之间协调变形程度增加,裂纹形核延迟,对裂纹扩展的阻碍作用增加,从而显著降低了韧脆转变温度。

关键词: 2.25Cr-1Mo-0.25V钢焊缝金属, 焊后热处理, 低温冲击韧性, 高温冲击韧性, 韧脆转变温度

Abstract: 2.25Cr1Mo0.25V steel is widely used in hydrogenation equipment and high-temperature, high-pressure pipelines due to its excellent high-temperature performance, tempering resistance, and high-temperature durability. However, its weld metal during welding is prone to issues such as uneven microstructure and high brittle ductile transition temperature, which can directly affect the safety and reliability of welded structural components under low-temperature or variable-load conditions. Therefore, in-depth research on the microstructure control and toughness improvement mechanisms of its weld metal is of great significance for the long-term stable operation of this material in large-scale equipment. The microstructure of three weld metal (as-welded (AW) and two post-weld heat treatments(PWHT) (705 ℃×8 h, PWHT.MIN) and 705 ℃×32 h, PWHT.MAX)) is characterized by scanning electron microscopy (SEM) and electron backscatter diffraction (EBSD). And the impact toughness of the weld metal is measured through the standard Charpy V-notch impact experiments in high/low temperature environments. The results indicate that the microstructure of AW specimen primarily consists of blocky ferrite and granular bainite, exhibiting microstructure inhomogeneity and incoordination of deformation between grains, and the impact energy at 25 ℃ is less than 10 J; while after holding at 200 ℃ for 20 minutes, ferrite appears in the microstructure, and the impact energy reaches 90 J. After post-weld heat treatment, the microstructure is composed of ferrite, and the impact energy at 25 ℃ is increased to 200 J. The brittle ductile transition temperatures of the AW, PWHT.MIN, and PWHT.MAX specimens are 158 ℃, -30 ℃, and -40 ℃, respectively. As tempering time increases, the degree of coordinated deformation between grains improves, crack nucleation is delayed, and the resistance to crack propagation is enhanced, leading to a significant reduction in the brittle ductile transition temperature.

Key words: 2.25Cr-1Mo-0.25V steel weld metals, post weld heat treatment, low-temperature impact toughness, high-temperature impact toughness, ductile-to-brittle transition temperature