机械工程学报 ›› 2018, Vol. 54 ›› Issue (18): 42-48.doi: 10.3901/JME.2018.18.042

• 材料科学与工程 • 上一篇    下一篇

超临界流体辅助微孔发泡注塑技术及其熔体发泡行为

董桂伟, 赵国群, 管延锦, 王桂龙, 侯俊吉, 吴昊   

  1. 山东大学材料液固结构演变与加工教育部重点实验室 济南 250061
  • 收稿日期:2018-01-21 修回日期:2018-04-24 出版日期:2018-09-20 发布日期:2018-09-20
  • 作者简介:董桂伟,男,1981年出生,博士研究生。主要研究方向为微孔塑料成型工艺与技术。E-mail:gwdong@sdu.edu.cn;赵国群,男1962年出生,教授,博士研究生导师。主要研究方向为塑性成形理论、数值模拟方法、模具CAD/CAM/CAE。E-mail:zhaogq@sdu.edu.cn
  • 基金资助:
    山东省优秀创新团队(2012-136)、中国博士后科学基金(2018M632671)和材料成形与模具技术国家重点试验室开放课题研究基金(P2018-002)资助项目。

Supercritical Fluid Assisted Microcellular Injection Molding and the Melt Foaming Behaviors

DONG Guiwei, ZHAO Guoqun, GUAN Yanjin, WANG Guilong, HOU Junji, WU Hao   

  1. Key Laboratory for Liquid-Solid Structural Evolution and Processing of Materials of Ministry of Education, Shandong University, Jinan 250061
  • Received:2018-01-21 Revised:2018-04-24 Online:2018-09-20 Published:2018-09-20

摘要: 开发一种超临界流体辅助微孔发泡注塑新技术,研制相应的超临界流体发生与计量控制技术系统,构建超临界流体辅助微孔发泡注塑试验线,并对超临界流体辅助微孔发泡注塑熔体的发泡行为进行研究。结果表明,超临界流体辅助微孔发泡注塑熔体的发泡过程包括“填充过程中发泡”和“填充结束后发泡”两个过程,分别对应成型产品内部的变形椭球形泡孔和规则球形泡孔两种不同的泡孔结构形态,而熔体“填充过程中发泡”形成的泡孔,受熔体剪切和喷泉流动行为的影响而发生变形,并在熔体流动前锋处破裂、涌出,与冷的模具表面接触后冷凝遗留在产品表面,形成表面气泡痕。所揭示的发泡演变过程和缺陷产生机理对微孔发泡注塑工艺原理和质量控制有较高的参考意义和工程应用价值。

关键词: 超临界流体, 发泡行为, 熔体, 微孔发泡注塑技术

Abstract: A new supercritical fluid assisted microcellular injection molding technique and the corresponding supercritical fluid generation, measurement and monitoring systems are developed. The supercritical fluid assisted microcellular injection molding test line is constructed. The melt foaming behaviors in supercritical fluid assisted microcellular injection molding are investigated. The results show that the melt foaming process in supercritical fluid assisted microcellular injection molding contains two processes:"foam during injection" and "foam after injection", respectively corresponding to the two different cell morphologies of distorted ellipsoidal cells and the regular spherical cells in the microcellular injection molded parts. The cells formed in "foam during injection" process are stretched by the shear flow and fountain flow behaviors, then broken, pushed out and turned over to both sides of the melt flow front, and finally contacted with the cold mold cavity surface and solidified to form surface bubble marks on the molded parts. The revealed foaming processes and defects generation mechanism have higher reference significance and engineering application value for technological principle and quality control of microcellular injection molding.

Key words: foaming behavior, melt, microcellular injection molding, supercritical fluid