轮轨循环滚动接触下钢轨绝缘接头损伤研究

周志军1, 杨辰禹1, 郭涛2, 陶功权1, 温泽峰1   

  1. 1. 西南交通大学轨道交通运载系统全国重点实验室 成都 610031;
    2. 大连交通大学詹天佑学院(中车学院) 大连 116028
  • 收稿日期:2025-11-21 修回日期:2026-05-22 发布日期:2026-11-20
  • 作者简介:周志军,男,1993年出生,博士研究生。主要研究方向为轮轨滚动接触及损伤。E-mail:zhijunzhou128@163.com;温泽峰(通信作者),男,1976年出生,博士,研究员,博士研究生导师。主要研究方向为轮轨关系和振动噪声。E-mail:zfwen@swjtu.edu.cn
  • 基金资助:
    国家自然科学基金资助项目(U21A20167)。

Study on Damage of Insulated Rail Joints under Wheel-rail Cyclic Rolling Contact

ZHOU Zhijun1, YANG Chenyu1, GUO Tao2, TAO Gongquan1, WEN Zefeng1   

  1. 1. State Key Laboratory of Rail Transit Vehicle System, Southwest Jiaotong University, Chengdu 610031;
    2. Zhan Tianyou College (CRRC College), Dalian Jiaotong University, Dalian 116028
  • Received:2025-11-21 Revised:2026-05-22 Published:2026-11-20

摘要: 钢轨绝缘接头是铁路线路中重要的机械连接和电气绝缘部件,但也是最易发生损伤的薄弱部件。建立考虑绝缘接头结构和材料非连续性特征的三维轮轨循环滚动接触有限元模型,采用子结构缩减、车轮超单元和多子程序嵌套技术,实现高效模拟车轮循环滚动通过绝缘接头时的接触应力应变行为演化过程,分析绝缘接头损伤机制。结果表明,绝缘接头非连续性导致接头两侧钢轨表面接触压力与剪切应力分布突变,形成明显的应力集中与非对称性特征。车轮循环滚动后,轨缝右侧(迎轮侧)承受较高的等效应力与等效塑性应变,且塑性应变累积速率明显高于左侧(顺轮侧),易产生棘轮效应并诱发损伤。随着轮轨循环滚动次数和蠕滑率的增大,由塑性应变累积导致的接头错牙量与凹陷量逐渐增大,几何不平顺水平逐步恶化。

关键词: 钢轨绝缘接头, 疲劳损伤, 轮轨循环滚动接触, 有限元法, 棘轮效应

Abstract: Insulated rail joints(IRJs) are a critical component in rail track as they serve as both a mechanical connector and an electrical insulator; however, they are also one of the most susceptible components to damage. In this study, a three-dimensional finite element model of wheel-rail cyclic rolling contact is presented that accounts for the structural and material discontinuities in the IRJs. The model uses a substructure reduction, a wheel superelement, and several user subroutines to efficiently simulate the evolution of contact stresses and strains as the wheel roll through the IRJs, focusing on the damage mechanisms involved. The results show that the discontinuity of the IRJs leads to abrupt changes in the distribution of contact pressure and surface shear stress on the rail surfaces at the IRJs, resulting in significant stress concentrations and asymmetries. After the wheels roll, the right side of the IRJs is subjected to higher equivalent stress and equivalent plastic strain, with the accumulation rate of plastic strain being significantly higher than that on the left side, making it more susceptible to ratcheting effects and possible damage. As the number of wheel-rail rolling cycles and the creepage increase, the accumulated plastic strain leads to an increase in the height difference and rail depression, which progressively exacerbates the geometric irregularities and deterioration of the IRJs.

Key words: insulated rail joints, fatigue damage, wheel-rail cyclic rolling contact, finite element method, ratcheting

中图分类号: