Correlation between the Ductile Brittle Transition Behavior and the Coordinated Deformation of Adjacent Grains of Cr-Mo-V Steel Weld Metal
DOU Guishan1, CAO Rui1, QIAO Xiaoli2, JIANG Yong3, LI Yimin2, TAO Yanwen2, ZHANG Kejing3, LI Jinmei4, WANG Cen2, LIN Qiaoli1
1. Department of Materials Science and Engineering, Lanzhou University of Technology, Lanzhou 730050; 2. Lanzhou Ls Heavy Equipment Co., Ltd., Lanzhou 730050; 3. Sichuan Atlantic Welding Materials Co., Ltd., Zigong 643000; 4. Lanzhou Ls Testing Technology Co., Ltd., Lanzhou 730050
DOU Guishan, CAO Rui, QIAO Xiaoli, JIANG Yong, LI Yimin, TAO Yanwen, ZHANG Kejing, LI Jinmei, WANG Cen, LIN Qiaoli. Correlation between the Ductile Brittle Transition Behavior and the Coordinated Deformation of Adjacent Grains of Cr-Mo-V Steel Weld Metal[J]. Journal of Mechanical Engineering, 2026, 62(18): 339-347.
[1] CORINNE C,SCHMITT J P. Additional recommendations for welding Cr-Mo-V steels for petrochemical applications[J]. Welding in the World,2013,55(11-12):31-38. [2] PEREIRA P A S,FRANCO C S G,GUERRA F J L M,et al. Hydrogen effects on the microstructure of a 2.25Cr–1Mo–0.25V steel welded joint[J]. International Journal of Hydrogen Energy,2015,40(47):17136-17143. [3] TAKAUCHI H,NAKANISHI T,NAKO H. Welding consumables for 2.25Cr-1Mo-V refining reactors[C]// Proceedings of the ASME 2017 Pressure Vessels and Piping Conference,American Society of Mechanical Engineers,Waikoloa,Hawaii,USA,2017,7:1-10. [4] CARDENAS A L,SILVA R O,ECKSTEIN C B,et al. Hydrogen effect on 2.25Cr–1Mo–0.25V bainitic steel under aging heat treatment[J]. International Journal of Hydrogen Energy,2018,43(33):16400-16410. [5] ANTALFFY L P,CHAKU P N,CANONICO D A,et al. The potential for using high chromium ferritic alloys for hydroprocessing reactors[J]. International Journal of Pressure Vessels and Piping,2002,79(8-10):561-569. [6] CHAUVY C,PILLOT S. Prevention of weld metal reheat cracking during Cr-Mo-V heavy reactors fabrication[C]// Proceedings of the Asme Pressure Vessels & Piping Conference,American Society of Mechanical Engineers,Prague,Czech Republic, 2009:243-251. [7] SCHÖNMAIER H,KREMMER T,BRABETZ M,et al. High-resolution characterization of precipitates in multi-layer submerged-arc welded 2.25Cr-1Mo-0.25V steel[J]. Materials Today Communications,2022,31:103299. [8] ZERBST U,AINSWORTH R A,H. BEIER T,et al. Review on fracture and crack propagation in weldments:A fracture mechanics perspective[J]. Engineering Fracture Mechanics,2014,132:200-276. [9] SUN Jian,LU Shanping. Effect of inhomogeneity on the microstructural evolution and mechanical behaviour of a vanadium-containing Fe–Cr–Ni–Mo weld metal[J]. Materials Science and Engineering:A,2021,806:140758. [10] SUN Jian,LU Shanping. Influence of inter-dendritic segregation on the precipitation behaviour and mechanical properties in a vanadium-containing Fe–Cr–Ni–Mo weld metal[J]. Scripta Materialia,2020,186:174-179. [11] TAKAYAMA N,MIYAMOTO G,FURUHARA T. Chemistry and three-dimensional morphology of martensite-austenite constituent in the bainite structure of low-carbon low-alloy steels[J]. Acta Materialia,2018,145:154-164. [12] LI Xinyu,JIANG Yong,WU Kefan,et al. Effects of pre-tempering on the microstructure,hardness and impact toughness of the 2.25Cr–1Mo-0.25V heat-resistant steel weld metal[J]. International Journal of Pressure Vessels and Piping,2021,193:104455. [13] WANG Shyi-Chin,YANG Jer-Ren. Effects of chemical composition,rolling and cooling conditions on the amount of martensite/austenite (M/A) constituent formation in low carbon bainitic steels[J]. Materials Science and Engineering:A,1992,154(1):43-49. [14] ENDO S. The effect of applied thermal cycle conditions on chemistry and volume fraction of M-A constituent formed in a low alloy steel[J]. Tetsu-to-Hagane,1998,84(4):297-302. [15] BISS V,CRYDERMAN R L. Martensite and retained austenite in hot-rolled,low-carbon bainitic steels[J]. Metallurgical Transactions,1971,2(8):2267-2276.. [16] KIKUTA Y,ARAKI T,YONEDA M,et al. Effect of martensite-austenite constituent on fracture behavior of weld zone of HSLA steel[J]. Journal of the Society of Materials Science,Japan,1985,34(381):638-642. [17] DAVIS C L,KING J E. Cleavage initiation in the intercritically reheated coarse-grained heat-affected zone:Part I. Fractographic evidence[J]. Metallurgical and Materials Transactions A,1994,25(3):563-573. [18] SCHÖNMAIER H,KREIN R,SCHMITZ-NIEDERAU M,et al. Influence of the heat input on the dendritic solidification structure and the mechanical properties of 2.25Cr-1Mo-0.25V submerged-arc weld metal[J]. Journal of Materials Engineering and Performance,2021,30(10):7138-7151. [19] 蒋文春,罗云,万娱,等. 焊接残余应力计算、测试与调控的研究进展[J]. 机械工程学报,2021,57(16):306-328. JIANG Wenchun,LUO Yun,WAN Yu,et al. Research progress on the calculation,measurement and control of welding residual stress[J]. Journal of Mechanical Engineering,2021,57(16):306-328. [20] API Recommended Practice:934-A Materials and fabrication of 21/4CR–1Mo,21/4 Cr–1Mo–1/4V,3 Cr–1Mo and 3Cr–1Mo–1/4V steel heavy wall pressure vessels for high-temperature,high-pressure hydrogen service[R]. API Publishing Services,2008. [21] CHERUVU N S. Degradation of mechanical properties of Cr-Mo-V and 2.25Cr-1Mo steel components after long-term service at elevated temperatures[J]. Metallurgical Transactions A,1989,20(1):87-97. [22] WU Kefan,YAN Yingjie,CAO Rui,et al. Microstructure and charpy impact toughness of a 2.25Cr-1Mo-0.25V steel weld metal[J]. Materials (Basel),2020,13(13):3013. [23] KUMAR M,MISHRA S. Implications of the micromechanical Taylor factor on work hardening parameters:New perspectives from FFT simulations in DAMASK[J]. Computational Materials Science,2024,237:112892. [24] 姚顺语,马凤仓,刘平,等. 晶界工程处理对304奥氏体不锈钢力学性能的影响[J]. 有色金属材料与工程,2023,44(5):28-35. YAO Shunyu,MA Fengcang,LIU Ping,et al. Effect of grain boundary engineering processing on mechanical properties of 304 austenite stainless steel[J]. Nonferrous Metal Materials and Engineering,2023,44(5):28-35.