[1] WANG S,SONG L,KANG S,et al. Deformation behavior and microstructure evolution of wrought magnesium alloys[J]. Chinese Journal of Mechanical Engineering,2013,26(3):437-447. [2] 李落星,周佳,张辉. 车身用铝、镁合金先进挤压成形技术及应用[J]. 机械工程学报,2012,48(18):35-43. LI Luoxing,ZHOU Jia,ZHANG Hui. Advanced extrusion technology and application of aluminium,magnesium alloy for vehicle body[J]. Journal of Mechanical Engineering,2012,48(18):35-43. [3] DONG G,ZHAO C,PENG Y,et al. Hot granules medium pressure forming process of AA7075 conical parts[J]. Chinese Journal of Mechanical Engineering,2015,28(3):580-591. [4] SHEN D,CAI J,GUO C,et al. Evolution of residual stresses in micro-arc oxidation ceramic coatings on 6061 Al alloy[J]. Chinese Journal of Mechanical Engineering,2013,26(6):1149-1153. [5] CHANG H,ZHENG M Y,XU C. Microstructure and mechanical properties of the Mg/Al multilayer fabricated by accumulative roll bonding (ARB) at ambient temperature[J]. Materials Science and Engineering A,2012,543:249-256. [6] LIU H S,ZHANG B,ZHANG G P. Microstructures and mechanical properties of Al/Mg alloy multilayered composites produced by accumulative roll bonding[J]. Journal Material Science Technology,2011,27(1):15-21. [7] POURAHMAD P,ABBASI M. Materials flow and phase transformation in friction stir welding of Al 6013/Mg[J]. Transactions of Nonferrous Metals Society of China,2013(23):1253-1261. [8] LIU X B,CHEN R S,HAN E H,et al. Preliminary investigations on the Mg-Al-Zn/Al laminated composite fabricated by equal channel angular extrusion[J]. Journal of Materials Processing Technology,2009,209:4675-4681. [9] 柳绪静,刘黎明,王恒,等. 镁铝异种金属激光-TIG复合热源焊焊接性分析[J]. 焊接学报,2005,26(8):31-34. LIU Xujing,LIU Liming,WANG Heng,et al. Microstructure of laser-TIG hybrid welding joint of dissimilar metals of Al and Mg[J]. Transaction of the China Welding Situation,2005,26(8):31-34. [10] GAO Y,NAKATA K,NAGATSUKA K. Interface micro structural control by probe length adjustment in friction stir welding of titanium and steel lap joint[J]. Materials & Design,2015,65:17-23. [11] 郭训忠,陶杰,袁正,等. 爆炸焊接TA/AI复合管的界面及性能研究[J]. 稀有金属材料与工程,2012,41(1):139-142. GUO Xunzhong,TAO Jie,YUAN Zheng,et al. Investigation on interface and performance of explosive welded SS316L/Al clad tube[J]. Journal of Nanjing University of Aeronautics & Astronautics,2012,41(1):139-142. [12] HONARPISHEH M,ASEMABADI M,SEDIGHI M. Investigation of annealing treatment on the interfacial properties of explosive-welded Al/Cu/Al multilayer[J]. Materials & Design,2012,37:122-127. [13] ACARER M,GULENC B,FIDIK F. Investigation of explosive welding parameters and their effects on microhardness and shear strength[J]. Materials & Design,2003,24(8):659-664. [14] WRONKA B. Testing of explosive welding and welded joints: The microstructure of explosive welded joints and their mechanical properties[J]. Journal of Materials Science,2010,45(13):3465-3469. [15] 韩顺昌. 爆炸焊接界面相变与断口组织[M]. 北京:国防工业出版社,2011. HAN Shunchang. Phase transformation and fractography of interface of explosive welding[J]. Beijing:National Defence of Industry Press,2011. [16] XUE Q,GRAY G T. Development of adiabatic shear bands in annealed 316L stainless steel:Part II. TEM studies of the evolution of microstructure during deformation localization[J]. Metallurgical and Materials Transactions A,2006,37:2006-2447. [17] ACARER M,DEMIR B. An investigation of mechanical and metallurgical properties of explosive welded aluminium-dual phase steel[J]. Materials Letter,2008,62(25):4158. [18] MOUSAWI S,HASSANI S,ATKINS AG. Bond strength of explosively welded specimens[J]. Materials and Design,2008,29:1334-1352. [19] XIA H B,WANG S G,BEN H F. Microstructure and mechanical properties of Ti/Al explosive cladding[J]. Materials & Design,2014,56:1014-1019. [20] 王耀华. 金属板材爆炸焊接研究与实践[M]. 北京:国防工业出版社,2007. WANG Yaohua. Research and practice of explosive welding of metal plates[M]. Beijing:National Defence Industry Press,2007. [21] YAN Y B,ZHANG Z W,SHEN W. Microstructure and properties of magnesium AZ31B-aluminum7075 explosively welded composite plate[J]. Materials Science and Engineering A,2010,527:2241-2245. |